Yttria-stabilized tetragonal zirconia powders have been synthesized by reaction in molten salts at 450 °C. To obtain a Y2O3-ZrO2 solid solution powder, it was necessary to use yttrium salts (not yttrium oxide directly) in molten NaNO3-KNO3 eutectic. The agglomeration state of the powders depended on their washing conditions. An alcohol-washed powder containing soft agglomerates led to a fine-grained and high-density sintered body.

Dates et versions

hal-00754965 , version 1 (20-11-2012)

Identifiants

Citer

M. Descemond, Christian Brodhag, F. Thevenot, B. Durand, M. Jebrouni, et al.. Characteristics and sintering behaviour of 3 mol % Y2O3-ZrO2 powders synthesized by reaction in molten salts. Journal of Materials Science, 1993, Volume 28 (Issue 9), pp 2283-2288. ⟨10.1007/BF01151654⟩. ⟨hal-00754965⟩
75 Consultations
0 Téléchargements

Altmetric

Partager

More