TEM characterization of surface and crack oxidation of 316L SS in PWR water after hydrogenated-oxygenated cycles - Archive ouverte HAL Accéder directement au contenu
Communication Dans Un Congrès Année : 2023

TEM characterization of surface and crack oxidation of 316L SS in PWR water after hydrogenated-oxygenated cycles

Domaines

Matériaux
Fichier non déposé

Dates et versions

hal-04454788 , version 1 (13-02-2024)

Identifiants

  • HAL Id : hal-04454788 , version 1

Citer

Cecilie Duhamel, Thalita De Paula, Marc Maisonneuve, Catherine Guerre, Jérôme Crépin, et al.. TEM characterization of surface and crack oxidation of 316L SS in PWR water after hydrogenated-oxygenated cycles. 21st International conference on the environmental Degradation of Materials in Nuclear Power systems - Water reactors, Aug 2023, Newfoundland, Canada. ⟨hal-04454788⟩