Degradation of fluoride-free MIL-100(Fe) and MIL-53(Fe) in water: Effect of temperature and pH

Domaines

Chimie
Fichier non déposé

Dates et versions

hal-04238693 , version 1 (12-10-2023)

Identifiants

Citer

Igor Bezverkhyy, Guy Weber, Jean-Pierre Bellat. Degradation of fluoride-free MIL-100(Fe) and MIL-53(Fe) in water: Effect of temperature and pH. Microporous and Mesoporous Materials, 2016, 219, pp.117-124. ⟨10.1016/j.micromeso.2015.07.037⟩. ⟨hal-04238693⟩