Adhesive wear of a Ti6Al4V tribopair for a fast friction contact

Résumé

Friction tests at high sliding velocity are carried out by subjecting specimens to an apparent normal pressure of 110 MPa in the range of 40–64 m/s to reproduce severe conditions of contact between the rotating blades and the rotor in aircraft engines. Therefore, impacts of a projectile against a fixed sample are carried out for the investigation of a pair of Ti6Al4V materials. A mean coefficient of friction has been ascertained by two types of method: a tribometer device and an energetic approach. A slight sensitivity of the coefficient of friction with respect to the sliding velocity is observed. Postmortem analyses of samples reveal a decomposition of the frictional subsurface in multiple distinct layers: initial microstructure, severe plastic deformation (shear strain up to 16), phase transformation (View the MathML sourceT>980°C) and material transfer. A scenario of the adhesive wear mechanism is proposed in four steps.

Domaines

Matériaux
Fichier principal
Vignette du fichier
Chassaing2014.pdf (688.95 Ko) Télécharger le fichier
Origine Fichiers produits par l'(les) auteur(s)
Licence

Dates et versions

hal-01515223 , version 1 (23-09-2024)

Licence

Identifiants

Citer

Guillaume Chassaing, Laurent Faure, Sylvain Philippon, Mamadou Coulibaly, Albert Tidu, et al.. Adhesive wear of a Ti6Al4V tribopair for a fast friction contact. Wear, 2014, 320, pp.25-33. ⟨10.1016/j.wear.2014.08.001⟩. ⟨hal-01515223⟩
130 Consultations
0 Téléchargements

Altmetric

Partager

More