Compared activity and stability of three Ni-silica catalysts for methane bi- and dry reforming - Archive ouverte HAL
Article Dans Une Revue IEEE Transactions on NanoBioscience Année : 2015

Compared activity and stability of three Ni-silica catalysts for methane bi- and dry reforming

Résumé

A low weight % of Ni (5 wt %) and the two solvents technique of deposition are used to obtain well-dispersed Ni-species (either particles or species dispersed on the silica surface) and avoid the formation of large particles on three silicas SBA-15, Aerosil 300 and diatoms MN3. Stability tests at 650°C for valorization of methane obtained from natural or shale gas: methane dry reforming and at 800°C for bireforming are compared. For bireforming (steady state, 800°C, 10 h, CH4/CO2/H2O 1:0.4:0.8, 62,700 ml.g-1.h-1), an unexpected stability of Ni/Aerosil silica is observed and tentatively associated with the pretreatment applied to silica

Domaines

Chimie
Fichier non déposé

Dates et versions

hal-01264119 , version 1 (28-01-2016)

Identifiants

Citer

Karam Jabbour, M.N. Kaydouh, N El Hassan, H El Zakhem, Sandra Casale, et al.. Compared activity and stability of three Ni-silica catalysts for methane bi- and dry reforming. IEEE Transactions on NanoBioscience, 2015, pp.1-4. ⟨10.1109/MedGO.2015.7330318⟩. ⟨hal-01264119⟩
33 Consultations
0 Téléchargements

Altmetric

Partager

More