C. Rond, N. Derkaoui, M. Wartel, A. Tallaire, K. Hassouni, et al.. How to elaborate ultra pure diamond single crystal at high growth rate in MW-PACVD reactor. The XXXI International Conference on Phenomena in Ionized Gases (ICPIG) 2013, Jul 2013, Grenade, Spain. ⟨hal-01056905⟩