Tribological characterization of rail squat defects - Archive ouverte HAL Accéder directement au contenu
Article Dans Une Revue Wear Année : 2013

Tribological characterization of rail squat defects

Résumé

Rail squats remain a major rolling contact fatigue problem for mass transit authorities. Several studies have been conducted to supplement the standard characterization of rail squats. In particular an extensive tribological and metallurgical investigation was performed on samples of incipient squats from various areas. Surfaces and cross-sections of rail samples were observed by optical microscopy and scanning electron microscopy. These observations highlighted that the running band is composed of longitudinal contact strips with various surface and subsurface morphologies. This microstructure seems to be essential for the onset of squats. This new information makes it possible to account for the entire damage mechanism of a squat defect from initiation to propagation.

Dates et versions

hal-00764214 , version 1 (12-12-2012)

Identifiants

Citer

Samuel Simon, Aurélien Saulot, Camille Dayot, Xavier Quost, Yves Berthier. Tribological characterization of rail squat defects. Wear, 2013, 297, pp.926 - 942. ⟨10.1016/j.wear.2012.11.011⟩. ⟨hal-00764214⟩
164 Consultations
0 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More