Non-local fatigue criterion based on standard deviation for notches and defects in Ti-6Al-4V

Résumé

The aim of this study is to propose a non local multiaxial fatigue criterion in order to assess the fatigue limit of stress concentrator such as notches or defects in Ti-6Al-4V. This criterion is based on the standard deviation of the stresses integrated over a given volume around the hot spot point. Four parameters are necessary to identify the criterion. The criterion is first validated on notched samples based on literature results and shows very good results. A set of experimental tests is conducted on natural and artificial defects including clustering defects and demonstrates the flexibility and accuracy of the criterion.
Fichier principal
Vignette du fichier
Bodlet Non-local fatigue criterion.pdf (2.29 Mo) Télécharger le fichier
Origine Fichiers produits par l'(les) auteur(s)
Licence

Dates et versions

hal-04254054 , version 1 (23-10-2023)

Licence

Identifiants

  • HAL Id : hal-04254054 , version 1

Citer

Natan Bodlet, Rémi Amargier, Yves Nadot. Non-local fatigue criterion based on standard deviation for notches and defects in Ti-6Al-4V. 2023. ⟨hal-04254054⟩
84 Consultations
32 Téléchargements

Partager

Gmail Mastodon Facebook X LinkedIn More