Résumé

Polyimide is one of the most used polymer for electrical insulation in severe environment. For future aircrafts, polymer electrical insulation will be exposed to thermal constraints that can affect its physic- ochemical structure. Effects of thermal ageing are studied through their impact on the relaxational be- haviour. Thermal degradation impairs first the aromatic entities and lately the carbonyls. It is responsible for the strong acceleration of mobility observed for both localised βand γrelaxation modes. Both DMA and swelling test exhibit an acceleration of localized molecular mobility. However, as the local mobility is accelerated, the increase in heterogeneities visible through the evolution of the MWS polarisation brings up to light a change in the charge transport mechanism. The chain scission degradation mechanism, leads to a decrease of the density of deep traps. It explains the evolution of both the value of DC conductivity and its activation energy upon ageing.
Fichier principal
Vignette du fichier
Henri_27520.pdf (1.34 Mo) Télécharger le fichier
Origine : Fichiers produits par l'(les) auteur(s)

Dates et versions

hal-03164667 , version 1 (10-03-2021)

Identifiants

Citer

Victor Henri, Eric Dantras, Colette Lacabanne, Flavien Koliatene, Christophe Trebosc. Ageing of Polyimide under thermal stress: relaxationnal effects and charge transport. Polymer Degradation and Stability, 2021, 186, pp.109524. ⟨10.1016/j.polymdegradstab.2021.109524⟩. ⟨hal-03164667⟩
47 Consultations
299 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More