Erratum to ‘‘A 3D diamond detector for particle tracking’’ [Nuclear Instruments Methods A 786 (2015) 97–104]
Résumé
The publisher regrets
p 98,“The electrode yield, i.e. the fraction of electrodes produced with a continuous conducting path over the thickness of the diamondsample, was estimated by optical and electrical inspection and found to be9273%.”(Was“9270.3%”)
p101, Figure 8 of the paper misses the legend, corrected figure:
p103, Figure 13b) of the paper misses 3 blue bin entries (corner bins) of the four, only one entry is visible.