Elizabeth Chaumun, Jérôme Crépin, Cecilie Duhamel, Catherine Guerre, Eva Heripre, et al.. SCC crack initiation in nickel based alloy welds in hydrogenated steam at 400°C. 17th international conference on environmental degradation of materials in nuclear power systems - water reactors, Aug 2015, Ottawa, Canada. 19 p. ⟨hal-01236330⟩