Damage developed during high temperature deformation of magnesium alloys: a continuous 3D characterisation by X-ray micro tomography - Archive ouverte HAL Accéder directement au contenu
Communication Dans Un Congrès Année : 2013

Damage developed during high temperature deformation of magnesium alloys: a continuous 3D characterisation by X-ray micro tomography

Domaines

Matériaux
Fichier non déposé

Dates et versions

hal-00950637 , version 1 (21-02-2014)

Identifiants

  • HAL Id : hal-00950637 , version 1

Citer

P. Lhuissier, M. Scheel, L. Salvo, E. Boller, M. Di Michiel, et al.. Damage developed during high temperature deformation of magnesium alloys: a continuous 3D characterisation by X-ray micro tomography. THERMEC 2013, Dec 2013, Las Vegas, France. ⟨hal-00950637⟩