Linewidth-narrowing and intensity noise reduction of the 2nd order Stokes component of a low threshold Brillouin laser made of Ge10As24Se68 chalcogenide fiber - Archive ouverte HAL
Article Dans Une Revue Optics Express Année : 2012

Linewidth-narrowing and intensity noise reduction of the 2nd order Stokes component of a low threshold Brillouin laser made of Ge10As24Se68 chalcogenide fiber

Résumé

A compact second-order Stokes Brillouin fiber laser made of microstructured chalcogenide fiber is reported for the first time. This laser required very low pump power for Stokes conversion: 6 mW for first order lasing and only 30 mW for second order lasing with nonresonant pumping. We also show linewidth-narrowing as well as intensity noise reduction for both the 1st and 2nd order Stokes component when compared to that of the pump source.
Fichier principal
Vignette du fichier
HeyTow_optExp2012.pdf (423.81 Ko) Télécharger le fichier
Origine Fichiers éditeurs autorisés sur une archive ouverte
Loading...

Dates et versions

hal-00789411 , version 1 (18-02-2013)

Identifiants

Citer

Kenny Hey Tow, Yohann Léguillon, Schadrac Fresnel, Pascal Besnard, Laurent Brilland, et al.. Linewidth-narrowing and intensity noise reduction of the 2nd order Stokes component of a low threshold Brillouin laser made of Ge10As24Se68 chalcogenide fiber. Optics Express, 2012, 20 (26), pp.B104 - B109. ⟨10.1364/OE.20.00B104⟩. ⟨hal-00789411⟩
204 Consultations
250 Téléchargements

Altmetric

Partager

More