Operando kinetics of hydrogen evolution and elemental dissolution I: The dissolution of galvanized steel in hydrochloric acid - UFR de Chimie de Sorbonne-Université Accéder directement au contenu
Article Dans Une Revue Corrosion Science Année : 2023

Operando kinetics of hydrogen evolution and elemental dissolution I: The dissolution of galvanized steel in hydrochloric acid

Résumé

A new approach to the simultaneous measurement of the hydrogen evolution reaction (HER) and elemental dissolution rates is presented and applied to the reaction of galvanized steel coatings with HCl solution. Dissolution profiles revealed several kinetic regimes including the dissolution of the intact coating, the dissolution of the nanometric Fe 2 Al 5 intermetallic layer, and the corrosion of the steel substrate. The HER and Zn dissolution rates were in excellent agreement, and the quantities of interfacial Fe and Al were consistent with the predicted 50 nm thick Fe 2 Al 5 intermetallic film, demonstrating the analytical capabilities of the atomic emission spectroelectrochemistry (AESEC) technique.
Fichier principal
Vignette du fichier
Dou_Operando kinetics of H2 evolution and elemental dissolution part I.pdf (3.29 Mo) Télécharger le fichier
Origine : Fichiers produits par l'(les) auteur(s)

Dates et versions

hal-03969836 , version 1 (02-02-2023)

Identifiants

Citer

Baojie Dou, Xuejie Li, Junsoo Han, Kevin Ogle. Operando kinetics of hydrogen evolution and elemental dissolution I: The dissolution of galvanized steel in hydrochloric acid. Corrosion Science, 2023, 214, pp.111007. ⟨10.1016/j.corsci.2023.111007⟩. ⟨hal-03969836⟩
14 Consultations
50 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More